Incoloy 925
Features:
Incoloy 925 is a precipitation-hardenable nickel-iron-chromium alloy. It combines high strength with Incoloy 825’s excellent corrosion resistance. Incoloy 925 is particularly resistant to sulfide-induced stress cracking and stress-corrosion cracking.

Applications:

Down-hole and surface well components for sour (containing hydrogen sulfide) crude oil and natural gas production.


Chemical composition:

% Ni Fe Cr C Mn Si P S Mo Cu Ti Al Nb
Min 42.0 22.0 19.5 2.5 1.5 1.9 0.10
Max 46.0 22.5 0.030 1.00 0.50 0.030 0.030 3.5 3.0 2.4 0.50 0.50

Physical properties:
Density 8.08 g/cm3
Melting range 1311-1366℃
Product Catalog